| dc.contributor.author | Kibona, Talam E. | |
| dc.contributor.author | Shao, Godlisten N. | |
| dc.contributor.author | Kim, Hee T. | |
| dc.contributor.author | King’ondu, Cecil K. | |
| dc.date.accessioned | 2019-02-04T13:32:14Z | |
| dc.date.available | 2019-02-04T13:32:14Z | |
| dc.date.issued | 2019-02 | |
| dc.identifier.citation | Nano-Structures & Nano-Objects Volume 17, Pages 21-33 | en_US |
| dc.identifier.issn | 2352-507X | |
| dc.identifier.uri | https://reader.elsevier.com/reader/sd/pii/S2352507X18302397?token=AFBEE7221BD710757E1DA39C75C38742A9E32A31429A7EEB987D5301E2FABCB325CE1610BBA775CBCC204385BBEA6E1B | |
| dc.identifier.uri | http://repository.seku.ac.ke/handle/123456789/4339 | |
| dc.description | DOI: https://doi.org/10.1016/j.nanoso.2018.10.002 | en_US |
| dc.description.abstract | Here, we report synthesis of biogas slurry mesoporous carbon/MnO composites by simple co-precipitation route followed by thermal treatment at 250 °C for 6 h. The texture, morphology, crystal structure, and microstructure of the composites are investigated by nitrogen sorption studies, FESEM, HRTEM, X-ray diffraction, and Raman spectroscopy. All samples exhibit type IV isotherms. The BET surface area decreased from 514 to 110 m2 g while total pore volume decreased from 0.52 to 0.17 cm g for samples loaded with and moles of Mn. The electrodes fabricated exhibit high specific capacitance of 709 F g−1 at scan rate of 5 mV s−1. The specific capacitance at scan rate of 5 mV s−1 increases with increasing MnO2 content. However, at 50 mV s−1, specific capacitance decreases with increasing MnO2 content. Varying the MnO2 content and hence the textural parameters, strongly influences the specific capacitances of the composite electrodes. | en_US |
| dc.language.iso | en | en_US |
| dc.publisher | Elsevier | en_US |
| dc.subject | Biogas slurry | en_US |
| dc.subject | Mesoporous carbon | en_US |
| dc.subject | Manganese oxide | en_US |
| dc.subject | Supercapacitors | en_US |
| dc.subject | Specific capacitance and composites | en_US |
| dc.title | Specific capacitance–pore texture relationship of biogas slurry mesoporous carbon/MnO2 composite electrodes for supercapacitors | en_US |